Good price  online

products details

Created with Pixso. Home Created with Pixso. Products Created with Pixso.
Hastelloy Alloy
Created with Pixso. 690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking

690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking

Brand Name: Runlai
Model Number: C4
MOQ: 2kg
Price: Negotiable
Delivery Time: 20~40 Days
Payment Terms: L/C, T/T, Western Union,
Detail Information
Place of Origin:
China
Certification:
CE,ROHS,ISO 9001
Product Name:
Hastelloy C4 Pipe
Material:
Ni Cr Mo
Elongation (≥ %):
40 %
Density:
8.89 G/cm3
Brinell Hardness HB:
≤220
Tensile Strength:
690 MPA
Yield Strength:
276 MPa
Application:
Engine Components And Combustion Chamber
Melting Point:
1330-1380°C
Thermal Conductivity:
9.4 W/m-K
Packaging Details:
Packed in Spool Carton box, Coil package with polybag,then in woodencase
Supply Ability:
300 tons per month
Highlight:

690 MPA hastelloy pipe

,

C4 hastelloy pipe

,

690 MPA hastelloy tube

Product Description

Chemical Processing Industry Hastelloy C4 Pipe 690 MPA Resistant To Stress Corrosion Cracking


Product Introduction


Hastelloy C4 pipe is a high-performance nickel-based alloy pipe with excellent corrosion resistance and high temperature stability, which is widely used in the chemical processing industry. Its main chemical components include nickel (Ni) 60-70%, chromium (Cr) 14-18%, molybdenum (Mo) 14-17%, iron (Fe) 3-7%, etc. These components give it excellent tolerance to a variety of acidic media, chlorides and other corrosive media in oxidizing and reducing environments. The physical properties of Hastelloy C4 pipe include density 8.64 g/cm³, melting point 1325-1370°C, tensile strength 760 MPa, yield strength 345 MPa, and elongation 50%. This alloy pipe can still maintain good mechanical properties and oxidation resistance in high temperature environments, and is suitable for the manufacture of chemical reactors, heat exchangers, distillation towers and other equipment. It has good processing performance and can be formed by conventional welding, cold rolling, hot rolling and other processes, and is suitable for the manufacture of parts with complex structures. Hastelloy C4 pipe has strict implementation standards and complies with ASTM B575 and ASME SB575 standards, ensuring its wide application in chemical, petroleum, aerospace and other fields.

 

Parameter


Hastelloy Alloy Ni Cr Co Mo FE W Mn C V P S Si
C-4 Balance 14-18 2 Max 14-17 3.0 Max   1.0 Max 0.015 Max   0.04 Max 0.03 Max 0.08 Max

 

  • Type we could offer
ASTM Alloy Type UNS Misc./Shape
ASTM B574
Bar
Hastelloy C-4 Nickel N06455 Bar
ASTM B575
Plate
Hastelloy C-4 Nickel N06455 Plate
ASTM B575
Strip
Hastelloy C-4 Nickel N06455 Strip
ASTM B575
Sheet
Hastelloy C-4 Nickel N06455 Sheet
ASTM B619
Welded Pipe
Hastelloy C-4 Nickel N06455 Welded Pipe
ASTM B622
Seamless Tubing
Hastelloy C-4 Nickel N06455 Seamless Tubing
ASTM B366
Fittings
Hastelloy C-4 Nickel N06455 Fittings
ASTM B574
Wire
Hastelloy C-4 Nickel N06455 Wire

 

Specific Applications


  1. Reactors and Agitators: Used in the manufacture of reactors and agitators that handle corrosive chemicals such as strong acids, such as sulfuric acid, hydrochloric acid, acetic acid, etc. Hastelloy C4 performs well in these environments and is able to resist uniform corrosion and stress corrosion cracking.
  2. Piping Systems: Used in piping systems for the transportation of corrosive chemicals, its good corrosion resistance and welding properties make it an ideal material choice.

 

Advantages and Characteristics


  • High strength and toughness: Hastelloy C4 pipe has a tensile strength of 650 MPa, a yield strength of 280 MPa, and an elongation of 40%. It has high strength and good toughness and can withstand large operating pressures and temperatures.
  • Good ductility: It has good ductility and is easy to process and form, suitable for various processing processes such as forging, hot rolling, cold working and welding.
  • Good machinability: Hastelloy C4 pipe has good machinability and can be forged, hot upsetting and impact extruded by a variety of methods. Although the alloy is easily work-hardened, it can be successfully spun, deep drawn, pressed or punched after proper treatment.
  • Excellent weldability: Hastelloy C4 pipe can be welded by various welding processes such as tungsten electrode inert gas shielded welding, plasma arc welding, manual sub-arc welding, metal inert gas shielded welding and melt inert gas shielded welding. For the best welding results, it is recommended to use pulse arc welding and ensure that the material is in an annealed state before welding.

 

Contact Us

Email:fbwlau@cnrunlai.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

 

Q&A


How does Hastelloy C4 pipe compare to Hastelloy C276 pipe?
Hastelloy C4 performs well in strong acid environments such as hydrochloric acid and sulfuric acid, while Hastelloy C276 performs better in environments such as wet chlorine and hypochlorite.

 

What specifications can Hastelloy C4 pipe be customized?
Hastelloy C4 pipe can be customized with different outer diameters, wall thicknesses and lengths to meet specific needs.

 

How is Hastelloy C4 pipe packaged?
Hastelloy C4 pipe is usually packaged in wooden or iron boxes to ensure safe transportation and storage.

 

What is the high temperature resistance of Hastelloy C4 pipe?
Hastelloy C4 pipe can maintain good performance in high temperature environments and is suitable for high temperature corrosive environments.

 

690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking 0690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking 1

Good price  online

Products Details

Created with Pixso. Home Created with Pixso. Products Created with Pixso.
Hastelloy Alloy
Created with Pixso. 690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking

690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking

Brand Name: Runlai
Model Number: C4
MOQ: 2kg
Price: Negotiable
Packaging Details: Packed in Spool Carton box, Coil package with polybag,then in woodencase
Payment Terms: L/C, T/T, Western Union,
Detail Information
Place of Origin:
China
Brand Name:
Runlai
Certification:
CE,ROHS,ISO 9001
Model Number:
C4
Product Name:
Hastelloy C4 Pipe
Material:
Ni Cr Mo
Elongation (≥ %):
40 %
Density:
8.89 G/cm3
Brinell Hardness HB:
≤220
Tensile Strength:
690 MPA
Yield Strength:
276 MPa
Application:
Engine Components And Combustion Chamber
Melting Point:
1330-1380°C
Thermal Conductivity:
9.4 W/m-K
Minimum Order Quantity:
2kg
Price:
Negotiable
Packaging Details:
Packed in Spool Carton box, Coil package with polybag,then in woodencase
Delivery Time:
20~40 Days
Payment Terms:
L/C, T/T, Western Union,
Supply Ability:
300 tons per month
Highlight:

690 MPA hastelloy pipe

,

C4 hastelloy pipe

,

690 MPA hastelloy tube

Product Description

Chemical Processing Industry Hastelloy C4 Pipe 690 MPA Resistant To Stress Corrosion Cracking


Product Introduction


Hastelloy C4 pipe is a high-performance nickel-based alloy pipe with excellent corrosion resistance and high temperature stability, which is widely used in the chemical processing industry. Its main chemical components include nickel (Ni) 60-70%, chromium (Cr) 14-18%, molybdenum (Mo) 14-17%, iron (Fe) 3-7%, etc. These components give it excellent tolerance to a variety of acidic media, chlorides and other corrosive media in oxidizing and reducing environments. The physical properties of Hastelloy C4 pipe include density 8.64 g/cm³, melting point 1325-1370°C, tensile strength 760 MPa, yield strength 345 MPa, and elongation 50%. This alloy pipe can still maintain good mechanical properties and oxidation resistance in high temperature environments, and is suitable for the manufacture of chemical reactors, heat exchangers, distillation towers and other equipment. It has good processing performance and can be formed by conventional welding, cold rolling, hot rolling and other processes, and is suitable for the manufacture of parts with complex structures. Hastelloy C4 pipe has strict implementation standards and complies with ASTM B575 and ASME SB575 standards, ensuring its wide application in chemical, petroleum, aerospace and other fields.

 

Parameter


Hastelloy Alloy Ni Cr Co Mo FE W Mn C V P S Si
C-4 Balance 14-18 2 Max 14-17 3.0 Max   1.0 Max 0.015 Max   0.04 Max 0.03 Max 0.08 Max

 

  • Type we could offer
ASTM Alloy Type UNS Misc./Shape
ASTM B574
Bar
Hastelloy C-4 Nickel N06455 Bar
ASTM B575
Plate
Hastelloy C-4 Nickel N06455 Plate
ASTM B575
Strip
Hastelloy C-4 Nickel N06455 Strip
ASTM B575
Sheet
Hastelloy C-4 Nickel N06455 Sheet
ASTM B619
Welded Pipe
Hastelloy C-4 Nickel N06455 Welded Pipe
ASTM B622
Seamless Tubing
Hastelloy C-4 Nickel N06455 Seamless Tubing
ASTM B366
Fittings
Hastelloy C-4 Nickel N06455 Fittings
ASTM B574
Wire
Hastelloy C-4 Nickel N06455 Wire

 

Specific Applications


  1. Reactors and Agitators: Used in the manufacture of reactors and agitators that handle corrosive chemicals such as strong acids, such as sulfuric acid, hydrochloric acid, acetic acid, etc. Hastelloy C4 performs well in these environments and is able to resist uniform corrosion and stress corrosion cracking.
  2. Piping Systems: Used in piping systems for the transportation of corrosive chemicals, its good corrosion resistance and welding properties make it an ideal material choice.

 

Advantages and Characteristics


  • High strength and toughness: Hastelloy C4 pipe has a tensile strength of 650 MPa, a yield strength of 280 MPa, and an elongation of 40%. It has high strength and good toughness and can withstand large operating pressures and temperatures.
  • Good ductility: It has good ductility and is easy to process and form, suitable for various processing processes such as forging, hot rolling, cold working and welding.
  • Good machinability: Hastelloy C4 pipe has good machinability and can be forged, hot upsetting and impact extruded by a variety of methods. Although the alloy is easily work-hardened, it can be successfully spun, deep drawn, pressed or punched after proper treatment.
  • Excellent weldability: Hastelloy C4 pipe can be welded by various welding processes such as tungsten electrode inert gas shielded welding, plasma arc welding, manual sub-arc welding, metal inert gas shielded welding and melt inert gas shielded welding. For the best welding results, it is recommended to use pulse arc welding and ensure that the material is in an annealed state before welding.

 

Contact Us

Email:fbwlau@cnrunlai.com

Oem service:
Welcome customized size
We are experience factory for OEM&ODM service

 

 

Q&A


How does Hastelloy C4 pipe compare to Hastelloy C276 pipe?
Hastelloy C4 performs well in strong acid environments such as hydrochloric acid and sulfuric acid, while Hastelloy C276 performs better in environments such as wet chlorine and hypochlorite.

 

What specifications can Hastelloy C4 pipe be customized?
Hastelloy C4 pipe can be customized with different outer diameters, wall thicknesses and lengths to meet specific needs.

 

How is Hastelloy C4 pipe packaged?
Hastelloy C4 pipe is usually packaged in wooden or iron boxes to ensure safe transportation and storage.

 

What is the high temperature resistance of Hastelloy C4 pipe?
Hastelloy C4 pipe can maintain good performance in high temperature environments and is suitable for high temperature corrosive environments.

 

690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking 0690 MPA Chemical Processing Industry C4 Hastelloy Pipe Resistant To Stress Corrosion Cracking 1